BaF2 Optical Crystals for Cross Polarized Wave Generation
← Back to product family

BaF2 Optical Crystals for Cross Polarized Wave Generation SKU: 540-7130

Cross-Polarized Wave (XPW) generation is a nonlinear third order process during which fundamental and generated waves have the same frequency; however, generated wave is perpendicularly polarized to pump wave polarization. Phase matching occurs over large bandwidth in XPW…

Variant specifications

Specification Value
Orientation [011]
Thickness 3 mm
Size 10x10 mm
Group Unmounted BaF2 Optical Crystals

Shared product specifications

These specifications apply across the BaF2 Optical Crystals for Cross Polarized Wave Generation product family.

Specifications

Material BaF₂
Surface quality 60-40 scratch & dig (MIL-PRF-13830B)
Clear aperture 90% of diameter
Diameter tolerance +0.0 -0.25 mm
Thickness tolerance 0.2 mm
Parallelism 3 arcmin
Flatness λ / 2 @ 633 nm
BaF₂ CaF₂ CVD-Diamond
Orientation h-cut [011] h-cut [011] z-cut [001]
Length, mm 2 2 1.2
n 1.464 1.426 2.383
(10⁻²² m² / V²) 1.53 0.94 11
σ -1.2 -0.6 -1.8
GVD (fs² / mm) -6 -27 63

Physical Properties

Crystal type cubic
Density, g / cm³ 5.27
Melting point, °C 1525
Refractive index @ 0.265 µm n = 1.51217
Refractive index @ 10.3 µm n = 1.39636
Transmission band, µm 0.135-15

Classification

Line femtoline

Product brochures

Shared documentation for the complete product family.